What are the qualified standard parameters for anodic oxidation of aluminum profiles?

1) Film thickness of 5-25um, hardness of 200HV or more, sealing test color change rate is less than 5%

2) Salt spray test in 36 hours or more, and can achieve more than 9 levels of CNS standards.

3) Appearance can not have bruises, scratches, color clouds and other phenomena. The surface can not have hanging points, yellowing and other bad phenomena].