Chemical composition of HPM75 nonmagnetic steel;
HPM75 nonmagnetic die steel contains 80% chemical elements.
C, Si, Mn, Cr, Mo, V and Al
0.65-0.75 0.80 15- 17 2-2.5 0.5-0.8 1.5-2 0.5-0.8 2.7-3.3
Properties of HPM75 nonmagnetic steel;
1. High strength
2. Ultra low permeability
3. Non-magnetic
4. High hardness
5. Wear resistance
6. No rust
7. Long service life
8. Stable chemical composition
9. Corrosion resistance
Application of HPM75 nonmagnetic steel;
1.HPM75 steel is suitable for mirror polishing molds, dust covers, TV filter plates, cosmetic boxes, transparent food boxes, etc.
2.HPM75 material is suitable for EDM die.
3.HPM75 material is suitable for precision corrugated molds, office automation equipment and auto parts.
Hardness of HPM75 nonmagnetic steel;
Ex-factory hardness: 300HBW, 450HBW
Nitriding hardness: 65HRC
Supply of HPM75 nonmagnetic steel:
In annealed and pre-hardened state, the scale on the surface of round steel and steel plate.
Heat treatment and metallographic structure of HPM75 nonmagnetic steel;
Heat treatment process of HPM75: solid solution1150-1180℃ water cooling; Aging at 650-700 DEG C; Air cooling, hardness 43-45HRC.
HPM75: Metallographic Structure of Austenite
The heat treatment parameters are as follows: HPM75 high temperature softening annealing heating temperature℃
Holding time/hour
Cooling mode
Hardness /HRC
870-890
three
furnace cooling
28-32
Solution aging treatment of HPM75
Solution temperature/℃
1 150- 1 180
Holding time/hour
15-20 (salt furnace)
cooling medium
water
Hardness /HRC
20-24
Aging temperature/℃
700
Holding time/hour
2
cooling medium
air-cooling
Hardness /HRC
248